Kev lag luam yog dominated los ntawm Aluminosilicate (xws li, Corning Gorilla, AGC Dragontrail) vim nws qhov siab compressive kev nyuaj siab.

 

Chemical Strengthening (ion{0}} pauv hauv KNO₃ da dej) yog tus qauv, ntsuas los ntawm DOL (qhov tob ntawm txheej) thiab CS (Compressive Stress).

 

Tsis zoo li thermal tempering, qhov no tso cai rau sub-0.5mm ultra-thin substrates tseem ceeb rau foldables thiab wearables.