Kev ntsuas lub kaum sab xis ntub dej thiab qhov nws qhia tau tiag tiag rau koj
Apr 07, 2026
Txhua AF txheej spec daim ntawv suav nrog lub kaum sab xis ntawm dej. Feem ntau cov neeg yuav khoom nod thiab txav mus. Qhov ntawd yog ib qho yuam kev.
Kev ntsuas lub kaum sab xis yog dab tsi
Muab ib tug tee dej deionized rau ntawm iav nto. Lub kaum sab xis ntawm ntug ntawm qhov poob thiab lub iav nto yog lub kaum sab xis ntawm kev sib cuag. Siab dua yog ntau hydrophobic (dej- ntxub). Lower yog ntau hydrophilic (dej-hlub).
Rau kev tiv thaiv- ntiv tes (AF) txheej, qhov chaw tshiab yuav tsum pom 110 txog 120 degrees. Uncoated iav zaum ntawm 30 txog 50 degrees. Cov roj ntiv tes rau ntawm cov iav tsis muaj coated kis tau tus kheej. Ntawm cov iav coated, nws hlaws thiab so tawm yooj yim.
Txoj kev dag tsis muaj leej twg qhia koj
Tiv tauj lub kaum sab xis nrog kev siv. Lub xov tooj tshiab qhia tau tias 115 degrees. Tom qab ib hlis ntawm kev siv ib txwm, nws poob rau 95 degrees. Tom qab 6 lub hlis, 70 txog 80 degrees. Qhov ntawd tseem siab dua cov iav uas tsis muaj coated. Tab sis oleophobic (roj-repelling) kev ua tau zoo twb degraded.
Qhov tseeb spec kom nug yog hu rau lub kaum ntse ntse tom qab puas. Standard test: 1cm x 1cm steel wool ncoo nrog 1kg load. So rov qab thiab tawm mus. Ntsuas txhua 1,000 lub voj voog.
Txheej zoo: nyob qis dua 100 degrees tom qab 5,000 cycles
Cov txheej txheem pheej yig: poob qis dua 80 degrees tom qab 2,000 lub voj voog
Txheej txheej pheej yig heev: ploj mus tom qab 1,000 cycles
Static vs. dynamic lub kaum sab xis
Lub kaum sab xis yog qhov poob zaum tseem. Dynamic lub kaum sab xis yog qhov poob txav thaum lub iav qaij. Qhov sib txawv ntawm lub kaum sab xis ua ntej (tej pem hauv ntej) thiab lub kaum sab xis (poob rov qab) yog hu ua hu rau lub kaum sab xis hysteresis. Lower hysteresis txhais tau hais tias lub txheej yog ntau yam.
Yog tias tus neeg muag khoom tsuas yog muab lub kaum sab xis rau koj, lawv tab tom zais qee yam. Nug cov ntaub ntawv hysteresis. Hauv qab 10 degrees yog qhov zoo heev. Tshaj 20 degrees txhais tau tias tsis zoo txheej txheej.
Cov neeg yuav khoom yuav tsum ua li cas
Yuav ib lub kaum sab xis tiv tauj lub ntsuas. Lawv raug nqi $500 txog $2,000. Ntsuam xyuas cov iav koj tus kheej. Tsis txhob tso siab rau cov ntawv pov thawj khoom muag. Peb tau pom daim ntawv pov thawj thov 115 degrees thaum qhov tseeb ntsuas 85 degrees tshiab tawm ntawm lub thawv.
Tsis tas li qhia qhov tsawg kawg nkaus lub kaum sab xis tom qab kev ntsuas kev puas tsuaj hauv koj daim ntawv cog lus yuav khoom. Yog tsis muaj qhov ntawd, koj tau txais kev ua tau zoo thawj zaug thiab cov neeg siv khoom npau taws rau lub hlis tom qab.