Kev lag luam nthuav dav ntawm npog iav

Apr 30, 2026

1.Lub ntsiab lus thiab daim ntawv thov

 

Lub npog iav, tseem hu ua npog lens yog pob tshab tiv thaiv txheej sab nraud ntawm lub vijtsam kov. Muaj ntau lub luag haujlwm: tiv thaiv khawb, tiv thaiv kev cuam tshuam, lub teeb hla thiab decroation.

Koj yuav pom nws siv hauv:

Cov khoom siv hluav taws xob (xov tooj, ntsiav tshuaj, smartwatches)
Automotive zaub (center consoles, instrument clusters)
Cov khoom siv kho mob, cov chaw ua lag luam, lub tsev facades, thiab lwm yam

 

2. Cov khoom siv tseem ceeb

Classified los ntawm tshuaj muaj pes tsawg leeg thiab ntxiv dag zog rau txoj kev:

Dej qab zib-lime iav - Tus nqi qis, kev ua haujlwm nruab nrab. Siv rau hauv cov khoom siv nyiaj txiag.

High-alumina iav (zoo li Corning's Gorilla Glass) - Tshuaj muaj zog. Nto compressive kev nyuaj siab (CS) siab tshaj 700 MPa, qhov tob ntawm txheej (DOL) tshaj 100μm.

Lithium-aluminosilicate iav - Siv ob- cov tshuaj ntxiv dag zog los txhawb CS thiab DOL tib lub sijhawm. Zoo dua poob tsis kam.

iav -ceramics - Cov khoom siv tshiab. Kev cuam tshuam zoo dua li cov iav aluminosilicate iav. Ntau lub xov tooj hauv Suav teb tau pib siv nws.

 

3. Cov txheej txheem tsim khoom

Rau 2D lossis 3D npog iav, cov kauj ruam ib txwm yog:

Raw khoom xaiv - Ultra- ntshiab lossis siab - alumina iav los xij, 0.4 txog 2.0mm tuab.

Txiav thiab CNC shaping - Txiav kom loj. Cov duab nyuaj (xws li 2.5D nkhaus npoo los yog lub koob yees duab qhov) xav tau siab - CNC precision kom tsis txhob ntug chipping.

Lapping thiab polishing - Tshem tawm burrs, du nto.

Tshuaj ntxiv dag zog - Ion pauv hauv cov poov tshuaj nitrate da dej. Tsim ib txheej CS siab, thawb hardness mus txog 7H.

Ntxuav - Ultrasonic da dej kom tshem tawm cov plua plav zoo.

Kev tshuaj ntsuam luam ntawv - Ntxiv cov logos, bezels, thiab lwm yam. Tshuab - luam tawm, kev sib haum xeeb nyob ib puag ncig ± 0.02mm.

Ink curing - Ci kom khi tus number case kom ruaj khov.

Kev kho deg - AG (anti-glare), AR (anti-reflection), AF (anti- ntiv tes).

Kev tshuaj xyuas thiab ntim khoom - Tshawb xyuas optics, qhov ntev, lub zog.

Ib qho ntxiv: 3D npog iav yuav tsum muaj qhov kub ntxiv -bending kauj ruam (700-750 degree, siv graphite pwm).

 

4. Cov thev naus laus zis tseem ceeb thiab kev tsim kho tshiab

Multi- chaw nres tsheb tshuaj ntsuam luam ntawv - A 2026 patent los ntawm Hunan Hewell Photoelectric (CN224159066U) siv lub phaj clamping nrog lub caij nplooj ntoos hlav hloov kom haum rau qhov sib txawv iav qhov ntau thiab tsawg, txhim kho kev luam ntawv raug.

Lub zeem muag alignment systems - Automates luam ntawv, hloov kev ua haujlwm ntawm phau ntawv, ua kom muaj txiaj ntsig zoo.

Ultra-thin flexible iav - nqes mus rau 0.03mm tuab rau cov ntaub ntawv foldable. Yuav tsum muaj cov cuab yeej ua kom nyias nyias. Heilongjiang Jintai Photoelectric yog tus thawj coj hauv tsev hauv qhov chaw no.

Kev sib xyaw ua ke - Kev sib xyaw txiav, CNC, luam ntawv, thiab tshuaj xyuas rau hauv ib qho kev ua haujlwm los txhawb kev ua haujlwm.

 

5. Kev lag luam toj roob hauv pes thiab tiam sis

Kev lag luam siab siab - Lens Technology thiab Biel Crystal yog ob lub tuam txhab Suav loj, ua ke ua ke feem ntau ntawm Apple thiab Samsung cov khoom siv.

Kev hloov pauv hauv tsev tau nrawm dua - Cov tuam txhab xws li CSG Holding, Iris Group, thiab Xuhong Optoelectronics tau ua tiav hauv siab - alumina substrates, tau los ze zog rau cov qauv thoob ntiaj teb.

Cov txheej txheem txheej txheem – Raw iav ntau lawm yog ob qho tib si thev naus laus zis- thiab peev- siv zog. Cov tuam txhab txawv teb chaws zoo li Corning tseem ua tus thawj coj siab kawg. Midstream processing yog ntau tshaj qhov teev thiab tawm los.

Qhov twg cov khoom mus rau -

Thinner thiab saj zawg zog (foldable zaub)

Smarter thiab ntau customized (AR/VR, automotive)

Ntau automation thiab digitalization

Koj Tseem Yuav Zoo Li