Ntug Chamfering Kev Paub hauv Npog iav Kev Lag Luam
Mar 30, 2026
Hauv kev lag luam npog iav, ntug chamfering yog ib qho tseem ceeb tshaj tawm - txheej txheem txheej txheem cuam tshuam rau cov khoom lag luam kev nyab xeeb, durability, zoo nkauj, thiab sib dhos ua ke. Nws grinds thiab polishes ntse txiav npoo rau hauv cov duab tshwj xeeb kom tshem tawm cov ntse, txo kev ntxhov siab, thiab ua tau raws li daim ntawv thov xav tau. Hauv qab no yog cov ntsiab lus luv luv ntawm cov hom chamfering, cov qauv kev ua haujlwm, thiab cov ntsiab lus tswj kom zoo raws li kev ua tau zoo.
1. Hom Edge Chamfering rau npog iav
Npog iav chamfering yog cais los ntawm cov duab, precision, thiab daim ntawv thov, nrog rau rau lub ntsiab hom raws li cov khoom yuav tsum tau.
1.1 Seamed Ntug
Qhov yooj yim tshaj plaws thiab tus nqi- hom zoo, feem ntau yog rau kev nyab xeeb los ntawm kev sib tsoo cov npoo du nrog ntxhib- pob zeb diamond log. Nws yog siv nyob rau hauv industrial tswj cov ntxaij vab tshaus, raws li ua ntej- ua rau siab -precision chamfers, thiab rau huab hwm coj-tsim, qis- zoo nkauj- xav tau cov khoom.
1.2 Flat Ntug
Av rau hauv ib qho ncaj, kab rov tav duab nrog ntau refined sib tsoo tshaj seamed npoo, kom ntseeg tau tias smoother nto thiab uniform thickness rau kev sib dhos zoo dua. Tsim nyog rau cov khoom lag luam, cov ntxaij vab tshaus soj ntsuam, thiab cov khoom siv hluav taws xob qis qis, feem ntau ua ke nrog yooj yim khawb- cov coatings resistant.
1.3 Pencil Edge
Lub npe rau nws cov cwj mem -zoo li lub voj voos, ntsuas kev nyab xeeb thiab kho kom zoo nkauj yooj yim. Ua tiav nrog emery- cov cuab yeej kos, nws yog siv hauv khw muag khoom kov cov ntxaij vab tshaus, rooj tog iav, thiab nruab nrab- cov khoom siv hluav taws xob, nrog lub vojvoog ntawm 0.5-2.0mm rau kev nplij siab thiab ruaj khov.
1.4 Beveled Ntug
Lub siab- hom zoo nkauj nrog 30℃-60℃kab pheeb ces kaum V-puab (1-}}5mm dav), yuav tsum muaj kev sib tsoo thiab polishing. Siv nyob rau hauv high-end electronics thiab coj mus muag zaub, ua tiav los ntawm CNC tshuab thiab polished rau ib daim iav tiav nrog cerium oxide.
1.5 2.5D Ntug
Mainstream nyob rau hauv cov neeg siv khoom siv hluav taws xob, nrog hloov maj mam nkhaus npoo (R0.3-R1.5mm) thiab qhov chaw tiaj tus. Nws txhim kho kev paub kov thiab kev zoo nkauj, siv hauv smartphones thiab hnav, ua tiav los ntawm CNC sib tsoo, polishing, thiab tiv thaiv tus ntiv tes txheej.
1.6 Kauj ruam Edge
Ib txheej txheej tshwj xeeb, ntaiv-zoo li chamfer, kho kom haum rau lub teeb pom kev zoo, tshwj xeeb- cov duab zoo li tus, thiab siab -kawg iav zoo nkauj. Nws yuav tsum tau siab - cov cuab yeej precision los xyuas kom meej cov kauj ruam tsis sib xws thiab kev hloov pauv, tsis txhob chipping.
2. Cov txheej txheem ua haujlwm tseem ceeb
Chamfering muaj peb theem txuas: sib tsoo, polishing, thiab tu, nrog kev sib txawv cuam tshuam rau qhov zoo.
2.1 Sib tsoo theem
Siv lub pob zeb diamond log (80 # -800 # grit rau ntxhib rau precision sib tsoo) los ua cov npoo. CNC tshuab ua kom muaj qhov sib xws, nrog ntau -axis tshuab rau cov chamfers tshwj xeeb.
2.2 Polishing theem
Tshem tawm kev sib tsoo khawb siv cov tshuaj txhuam hniav (cerium oxide, aluminium oxide) thiab cov cuab yeej muag muag. Ntau-theem polishing yog siv rau beveled / 2.5D npoo, thaum seamed / tiaj npoo yuav xav tau tsawg los yog tsis muaj polishing.
2.3 Theem Ntxuav
Tshem tawm cov seem ntawm ultrasonic tu, deionized dej yaug, thiab ziab. Plasma tu yog siv rau siab - daim ntawv thov precision los txhim kho qhov huv thiab adhesion.
3. Cov Ntsiab Cai Tswj Xyuas Zoo
Kev tswj nruj kom ntseeg tau zoo ib yam, tsom rau ob qhov tseem ceeb:
3.1 Dimensional Accuracy
Tswj lub kaum sab xis chamfer, dav, vojvoog, thiab thickness uniformity (xws li, ± 1℃rau bevel kaum sab xis, ± 0.05mm rau lub vojvoog). CMM tshuaj xyuas tsis tu ncua los kho cov tshuab tsis zoo.
3.2 Nto Zoo
Chamfers yuav tsum du, tsis muaj khawb, burrs, tawg, thiab residues -cov flaws no cuam tshuam rau kev nyab xeeb, durability, thiab tom qab ua tiav.