Npog iav Deep Dive: Dab tsi laser txiav tau hloov pauv
Apr 04, 2026
Cov neeg feem coob xav tias laser txiav tsuas yog huv dua li cov tshuab scribing. Qhov ntawd tsis yog tag nrho zaj dab neeg.
Yuav ua li cas mechanical script-thiab-break ua haujlwm
Lub pob zeb diamond lossis carbide log tau qhab nia ntawm iav nto. Qhov tob yog feem ntau 10-20 microns. Tom qab ntawd lub iav yog khoov raws cov qhab nia kab. Qhov tawg ua raws li tus sau ntawv. Yooj yim. Pheej yig. Ua haujlwm rau cov kab ncaj xwb.
Laser txiav txoj kev
Ob hom tseem ceeb yog siv niaj hnub no:
Filamentation (nthuav dav): Ib luv luv-mem tes laser tsim ib txoj hlua ntawm micro- qhov nyob rau hauv lub khob, tsis nyob rau saum npoo. Tom qab ntawd cov txheej txheem kev ntxhov siab los yog cov cua sov cais cov ntu. Tsis muaj deg khib nyiab. Tsis muaj ntug chipping.
CO2 laser nrog dej txias: Lub laser heats ib txoj kab nyias. Cov tshuaj tsuag dej txias tam sim ntawd. Thermal shock tsim kom huv si tawg. Qhov no yog sai dua filamentation tab sis tawm ntawm ntug rougher.
Qhov kev muag khoom tsis qhia koj
Laser txiav ua ib tug du ntug. Qhov ntawd yog qhov tseeb. Tab sis du tsis txhais hais tias muaj zog. Cov txheej txheem laser tawm micro- tensile stresses raws ntug txiav. Mechanical scribe yoojyim compressive stress. Compressive zoo dua rau kev poob qis.
Cov ntaub ntawv tiag tiag los ntawm 2025 tus neeg muag khoom tshawb xyuas: Tib iav, tib lub thickness. Mechanically scribed npoo muaj qhov nruab nrab flexural zog ntawm 480 MPa. Laser- txiav ntug (filamentation) ntsuas 410 MPa. Qhov ntawd yog 15% poob.
Thaum twg siv laser lawm
Cov duab tsis yooj yim. Mechanical script tsis tuaj yeem txiav cov nkhaus lossis qhov hauv. Laser tau. Kuj rau ultra- iav nyias (hauv qab 0.3mm). Mechanical script lov iav nyias yooj yim heev thaum sib cais. Laser yog softer.
Nqi kev muaj tiag
Laser txiav cov cuab yeej raug nqi 5-8x ntau dua li cov tshuab sau ntawv. Lub sij hawm voj voog kuj ntev dua. Rau siab - ntim ncaj txiav (xov tooj cov ntxaij vab tshaus, automotive center stacks), mechanical scribes tseem yeej ntawm tus nqi. Rau smartwatches, foldable sab hauv zaub, thiab lub koob yees duab npog qhov rais, laser yog tsim nyog tus nqi.